Most slabs-on-ground are unreinforced or nominally reinforced for crack-width control. When positioned ... random cracks that may occur because of concrete shrinkage and temperature restraints ...
When shrinkage stresses due to dry shrinkage and thermal contraction exceed the tensile strength of the concrete, cracking occurs. Contraction joints must already be in place to control the ...