"It uses common materials like sodium hydroxide—a common compound used ... In the next step, the porous mineral is treated with sulfuric acid and heated to 482 degrees Fahrenheit for two hours.
In this collage, from left, is: spodumene, the mineral concentrate containing the lithium to be extracted; spodumene roasted with sodium hydroxide ... treated with sulfuric acid and heated ...