Mayfair Gold Corp. ("Mayfair", "Mayfair Gold" or the "Company") (TSXV: MFG) (OTCQX: MFGCF) is pleased to provide an update on the recent results of the metallurgical test program conducted to advance ...
With a simple rougher-cleaner flotation process we are consistently able to produce an exceptionally clean, high-grade copper/gold concentrate with excellent metal recoveries and, significantly ...
Natural pH in the rougher circuit, collector dosage The copper rougher flotation tails leach flowsheet follows a typical copper flotation circuit configuration, with standard copper flotation ...
Copper Rougher Flotation Tails Leach: The copper rougher flotation tails leach flowsheet follows a typical copper flotation circuit configuration, with standard copper flotation reagents ...
The technology is not only limited to specific ore types, but also excels in various flotation applications, such as scavenger, rougher and cleaner circuits. “In scavenger applications ...
These latest results compared favorably with the first locked cycle test we announced on October 24, 2024. With a simple rougher-cleaner flotation process we are consistently able to produce an ...
The initial flotation rougher test results, Test F5, have shown a high rare earths recovery of 69.3% and good selectivity of rare-earth minerals, compared with fluorite. A review of the project's ...
A single multi-element ICP scan was conducted. A total of six rougher flotation tests were conducted on composite 4991-001, at feed sizes ranging from 80%-150µm to 80%-45µm, to evaluate response ...
Following grinding, the flotation plant will process the slurry with a prefloat stage before rougher copper flotation and a downstream nickel flotation circuit. The copper flotation circuit will ...
Rougher reagent collection and dosage was explored by seven flotation kinetics tests. The tests were run at fine grind of P80=106 μ to reduce mineral liberation effects. All tests were run at pH ...
Rougher Floatation Tests Two rougher flotation tests were conducted on the low grade BK2 composite. F01 applied an MF2 style flowsheet, where a flash flotation stage was conducted on the crushed ore ...